Boston MicroSystems (BMS)
Boston MicroSystems (BMS)BMS manufactures silicon carbide MEMS devices. Our SiC-based sensors have been demonstrated to work reliably at temperatures exceeding 500C for extended periods of operation. We can provide processed wafers, individual parts, or development systems for MEMS sensor and resonator design (including sampling system, control software.)