Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density4510 kg/m^3Solid DensityCRC Materials Science and Engineering Handbook, p.46
Specific heat522.5 J/kg/KAt Temp=25 C.CRC Materials Science and Engineering Handbook, p.261
Thermal conductivity21.9 W/m/KValue at temp=300 K.CRC Materials Science and Engineering Handbook, p.274-276
Young's Modulus115 GPaBulk material.Thin Solid Films,270(1995), p.263