MEMSnet Home: MEMS-Talk: Is there any way I can deposit gold onto pyrex wafer directly?
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-22
sokwon Paik
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-23
Gautham V
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-23
transene
Is there any way I can deposit gold onto pyrex wafer directly?
transene
2003-04-23
You may be able to electroplate gold onto Pyrex.  Transene offers the
RTM Process (Room Temperature Metallization) for depositing nickel onto
dielectric materials.  You could then deposit either electroless or
electrolytic gold on the nickel film.  Transene's plating solutions may
be viewed at www.transene.com, but feel free to contact me to discuss.

Christopher Christuk
Transene Company
10 Electronics Ave
Danvers MA  01923
Tel:  978 777 7860
Email:  [email protected]
-----Original Message-----
From: sokwon Paik [mailto:[email protected]]
Sent: Tuesday, April 22, 2003 12:37 PM
To: [email protected]
Subject: [mems-talk] Is there any way I can deposit gold onto pyrex
wafer directly?

I'm a student of Texas A&M University.
As far as I know, gold doesn't attach to pyrex glass
directly. But I think if I use sputtering machine then
it might be possible.
Anybody tried to attach gold directly onto pyrex
wafer?
One more question. Is there platinum sputtering source
exist?
If so, how much is it? Please answer me the question.
I appreciate your any reply.
Thanks,

sokwon Paik


__________________________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo
http://search.yahoo.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
The Branford Group