Allen Chou
2003-05-22
Justin Borski
2003-05-22
[email protected]
etch of tungsten oxide
[email protected]
2003-05-22
An argon plasma in an rie system works well for removing thin oxides. The
problem is when you remove it from the reactor it will immediately start to
oxidize again. What process step are you doing immediately after tungsten oxide
removal? Bob Henderson