Anodic bonding glass+aluminum+glass
2003-06-10
[email protected]
Anodic bonding glass+aluminum+glass
[email protected]
2003-06-10
Hi all,
I am trying to bond 1 micron thick aluming deposited on a  700 micron borofloat
glass to another glass wafer using anoding bonding technique.  I tried bonding
at 350C and 700 V , but it did not work.If anybody has done anything similar
and has any suggestions on the technique will be greatly appreciated.
Thanks
Gayathri


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review