A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: Mask Clean
RE: Mask Clean
2003-08-01
Jonathan Engel
RE: Mask Clean
Jonathan Engel
2003-08-01
I clean my chrome masks in an O2 plasma after an acetone/IPA/water/IPA rinse.
Regarding mylar masks, I would use IPA (or even acetone) on a soft cleanroom
wipe to gently wipe off organic contaminants, followed by a blow dry with dry
N2.

-Jon Engel