Ag wet etch
transene
2003-09-18
Transene Company offers Silver Etch TFS which will readily etch your
silver layer.  Please visit our website, www.transene.com, or contact me
directly.

Christopher Christuk
Transene Company
Tel:  978 777 7860
Email:  [email protected]

-----Original Message-----
From: Edward Keough [mailto:[email protected]]
Sent: Tuesday, September 16, 2003 11:57 AM
To: [email protected]
Subject: [mems-talk] Ag wet etch

Does anyone have a recommendation for wet etching a 100nm layer of
silver on a glass fiber. Through internet research I have only found a
recipe that calls for NH4OH:H2O2 (1:1) @ room temp, but no etch rate or
any other info. Does anyone have a recommendation. Thanks.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering