I use 5% Ammonium Chloride to wet etch a layer of ZnO. I was about to
modify the process by depositing a thin layer of aluminum before the ZnO
and was wondering if the Aluminum will get attacked by Ammonium
Chloride?

Thank you,
--
Shweta Humad