Dear Ravindra

Generally electroforming means the shape replication by electroplating.
If there is a material with certain shape, the metal is electroplated on the
material and then the material is removed or separated.
So a many methods can be used for electroforming.
If you tell me the structures you want to make,
I can say some proper methods for your study.

Sooje Cho from MEMSware


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.