> Greetings all, need advice.  How to minimize flash oxidation of
electroplated copper, are there any tricks or passivation agents?

> Thanks
> Rob Davis
> Caldus Semiconductor
> [email protected]

> Dear Rob,

Transene offers two products for copper oxide removal.  Transene COR-100
removes copper oxide films using a mild formulation.  Transene Bright Copper
Cleaner removes copper oxide and passivates the surface against further
oxidation.  Please visit our website at www.transene.com or contact me
directly.

Christopher Christuk
Transene Company
Tel:  978 777 7860
email:  [email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation