MEMSnet Home: MEMS-Talk: Thanks (RE: Q: Ti wet etching)
Thanks (RE: Q: Ti wet etching)
2003-10-22
t. hamano
Thanks (RE: Q: Ti wet etching)
t. hamano
2003-10-22
Hi.  Thanks for all who replied to my questions.
Since barium titanate film can be etched by HF (or BHF) solution, I am
trying the one with NH4OH.  The dry etch is one option and we will try once
the NH4OH effect to the material.

You guys are helpful!!

Sophie



reply