MEMSnet Home: MEMS-Talk: what about platinum over silicon dioxide?
what about platinum over silicon dioxide?
2003-10-23
Sebastian Sosin
2003-10-24
Kirt & Erika Zipf-Williams
2003-10-26
Elena Sidorov
what about platinum over silicon dioxide?
Elena Sidorov
2003-10-26
Ti or Cr is good choice

-----Original Message-----
From: Sebastian Sosin [mailto:[email protected]]
Sent: Thursday, October 23, 2003 10:19 PM
To: [email protected]
Subject: [mems-talk] what about platinum over silicon dioxide?


Do I need an adhesion layer before depositing platinum over silicon dioxide?


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics