MEMSnet Home: MEMS-Talk: process for SiC ecthing
process for SiC ecthing
2003-11-03
Chen-Han Lee
2003-11-05
Michael Huff
process for SiC ecthing
Chen-Han Lee
2003-11-03


Hi everyone,

I am releatively new to this area, so hope that you don't find my question
silly.
I would like to know the typical processes or chemicals I need for silicon
carbide(SiC) etching.

thanks very much in advance.



///////////////////////////////////
Chen-Han Lee
Research Student
School of Manufacturing and Mechanical Engineering,
University of Birmingham,
Birmingham, B15 2TT
United Kingdom,
Phone :  +44 121 4144245
Fax :    +44 121 4143958
E-Mail : [email protected]
///////////////////////////////////


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation