MEMSnet Home: MEMS-Talk: metal? etch mask for TMAH
metal? etch mask for TMAH
2003-10-29
Karin Buchholz
2003-10-30
Shile
2003-11-18
Martyna
2003-11-18
Massimiliano Decarli
2003-11-19
David Nemeth
SiO2 sputtering rate
2003-11-21
Oray Orkun Cellek
In search for another room-temp casting material on silicon
2003-11-18
Wei-han J. Wu
metal? etch mask for TMAH
Martyna
2003-11-18
Hello,

Does anybody know if gold mask can be used for TMAH etching? I have 1000 A gold
layer (with 100 A Cr) on a Si wafer. I used 5% TMAH and etch for half an hour.
The result is much below the typical etch rate.

Before etching I removed native oxide with HF.

Thank you for your help

Martyna
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer