I am working with SU8 in the visible range by adding photo initiator
sensitive to visible light.  Does any one know where can I get the raw
SU8 in solid form?
WY


--
Dr. Wing Yim Tam
Associate Professor
Physics Department
Hong Kong University of Science & Technology
Clear Water Bay
Hong Kong
Tel: 2358 7490
Fax: 2358 1652
email: [email protected]




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics