Hello All

I want to deposit electrodless nickel on a silicon wafer with Si02 on the
surface. From my literature review I have found this is done by sensitizing
the surface first with stanneous chloride or palladium chloride or both. I
currently don't have a good recipe so I am putting out this feeler to see if
anyone has any experience on this and could give me information about a
sensitizing recipe they use. For example a solution compositon, Immersion
times, stanneous/palladium chloride depositon rate, thickness necessary for
Nickel to adhere. Also I cannot find a supplier for the palladium chloride.
I have found companies that sell the solution in bulk but not in small
quantities which is what I need.

Any general information on platting Electrodless nickel on SiO2 would also
be appreciated
Thank You

Ahmed Shuja
Research Assistant
Center for Microelectronics and MEMS
University of Cincinnati

_________________________________________________________________
Cell phone ‘switch’ rules are taking effect — find out more here.
http://special.msn.com/msnbc/consumeradvocate.armx



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.