Hi everyone,
I want making a temperature sensor with Pt resistor. Can I diretly deposit Pt
onto Silicon?

I know about Pt doesn't adhere to silicon surface well. Generally, chromium is
used as the brazing metal layer between Pt and Silicon. However, if chromium
maybe make some bad effect on the linearity and sensitivity of the sensor or
not?

Gaofei Zhang
Precision Instrument and Mechanology Dept.
Tsinghua University, 100084,P.R.China
+86(10)62776000-805
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation
University Wafer