> Can Piranha etch both W and NiSi?

No certain etch rates, but:
H2O2 etches W, so Piranha should.
We tested Ni in Piranha and it etches. Si of course does not.
My guess is that NiSi will also be etched.
    --Kirt Williams, Ph.D.    consultant