MEMSnet Home: MEMS-Talk: tmah photoresit developer used to etch Si
tmah photoresit developer used to etch Si
2004-01-20
GuyHaché
2004-01-20
Neal Ricks
tmah photoresit developer used to etch Si
Neal Ricks
2004-01-20
Guy,

The concentration of TMAH as used in developer solution is typically too low to
effectively etch Silicon (at maybe 2%?).  You should try a chemical manufacturer
such as Aldrich, where you can get a pre-mixed solution that is a 24%
concentration.

Neal

Guy Haché  wrote:
Hi,

We have a bottle of tmah wich has photoresit developer written on it. Can we
use this tmah to etch Si?

Is it possible that there's additives in it which could diminish the etch rate?

Thank's

Guy Haché, M.Sc.A.
Assistant de recherche, research assistant
--------------------------------------------------------
Département de génie électrique et de génie informatique
Université de Sherbrooke
2500, boulevard Université
Sherbrooke (Québec) Canada
J1K 2R1
Téléphone/phone : (819) 821-8000 3706
Télécopieur/fax : (819) 821-7937
e-mail: [email protected]
--------------------------------------------------------

--------------------------------------------------------------------------------




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

---------------------------------
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.