MEMSnet Home: MEMS-Talk: Ti thin film resistivity
Ti thin film resistivity
2004-02-11
Anna Ohlander
2004-02-11
Kirt Williams
2004-02-11
MT Klaus Beschorner
Ti thin film resistivity
MT Klaus Beschorner
2004-02-11
 >Does anyone know where i can find info on the behaviour of the thin film
 >resistivity of Titanium.
 >Been searching the litterature but haven't had much success.

Versus which parameter? For as-deposited films, contamination is by far (by
REALLY far) the most important influence.
cheers,
klaus
--
Klaus Beschorner
Metron Technology Europe, PVD (Eclipse) Process Manager
Drosselweg 6,71120 Grafenau,Germany. Tel +49-7033-45683





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics