MEMSnet Home: MEMS-Talk: AZ4620
AZ4620
2004-02-14
[email protected]
2004-02-16
[email protected]
AZ 5214
2004-02-17
[email protected]
AZ4620
[email protected]
2004-02-16
HMDS is best done in a YES oven under controlled conditions. You might contact
Bill Moffet at Yield Engineering Services for better instruction.

It might be to no avail as the work we have done on our new silicon etch process
shows a selectivity of oxide to silicon of around 1:100. If the math is right
you will only be able to etch around 70 microns total before you run out of hard
mask material. You might need to thicken up the oxide and etch it with plasma to
insure proper wall angle before Silicon etch process. Bob Henderson


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
The Branford Group
Mentor Graphics Corporation