I am trying to open a 1x2 mm diaphragm to backside of a silicon wafer using
KOH. The backside is unpolished and this makes the deposited PECVD SixNy
weak to KOH. Any suggestion and experience about etching through a rough
surface will help.
Thanks
=================================

Isa Kiyat