About laser holography
2004-05-27
tao liu
2004-05-28
Bill Moffat
About laser holography
tao liu
2004-05-27
Hi,

I use HeCd laser to do holography with two-beam interference.  The
wavelength is 446nm.  My sample is PR1805/SiO2/GaAs.  The period is
1.5um.  The sample is exposed twice to form a crossed grating.  After
exposure and development, I can always see the non-uniformity on the
sample surface: some area has good exposure, some area has
under-exposure, and some area has over-exposure.  Because the time for
a single exposure is only ~ 3s and the development is also only ~ 3s,
I suspect that this is caused by the very short development time.  (I
cannot use long development time for my present conditions.  Otherwise
all the patterns will be lost.)  Can anybody give me some hints for
that?  Thanks.

Best regards,

Tao


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering