Silicon nitride membrane : wafer dicing problem
2004-07-06
Mahavir Sanghavi
2004-07-06
Shile
2004-07-06
Jim Beall
UV Cure of Thick Photoresist
2004-07-08
Eric Miller
2004-07-06
David Springer
Silicon nitride membrane : wafer dicing problem
David Springer
2004-07-06
Hi Mahvir

Is the membrane that is cracking released or is it cracking where it is attached
to the silicon. If it is the released area that is cracking then you might
consider releasing the membrane after dicing. If this would solve the problem I
can discuss with you how you can use XeF2 to remove the silicon under the
membrane while the diced wafer is still on the dicing tape.

David Springer
XACTIX, Inc.

>>  Hi all,

 >>  I am looking for a way to dice my silicon wafer with deep etched pockets
 >>  with a micron thick 8 mm by 8 mm silicon nitride membrane on one side. I
 >>  tried to use the wax to fill in the cavities and dice. But, I observed
 >>  the membranes break. Our dicing saw uses a high pressure water stream to
 >>  cool the diamond blade. I would appreciate if anyone has any suggestions.

 >>  Thanks in advance,
 >>  -Mahavir Sanghavi
 >>  _______________________________________________
 >>  [email protected] mailing list: to unsubscribe or change your list
 >>  options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
 >>  Hosted by the MEMS Exchange, providers of MEMS processing services.
 >>  Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review