MEMSnet Home: MEMS-Talk: Question about thermal conductive glue for drie
Question about thermal conductive glue for drie
2004-07-08
Han Geun Yu
2004-07-08
[email protected]
2004-07-09
Jobert van Eisden
2004-07-10
#GUO XUN#
2004-07-15
Xu Zhu
Question about thermal conductive glue for drie
Han Geun Yu
2004-07-08
Hi, I am struggling with heat problem of substrate while doing drie. Because I
use small piece, I need carrier wafer to do drie and I think it makes heat to
flow little. If you know any glue or greese to increase the heat flow, please
let me know.

Thank you.

Han
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.