Leidong Mao,
You do not need anything special, the power requirements depend on the area you
wish to plate.  In the mems world of very small dimensions you can use a small
metallurgical electropolisher.  You may want to stick a more sensitive meter,
(current and voltage) and a timer on the setup...

You may want to buy a commercial copper bath, sold at most hobby shops for under
$25.

good luck
Rob

>
> From: Leidong Mao 
> Date: 2004/07/26 Mon PM 10:17:17 GMT
> To: [email protected]
> Subject: [mems-talk] Power supply for copper
>
> Hello All,
>     We are looking for a power supply for copper
> electroplating setup. Could anyone please suggest a
> good P.S for this purpose? If possible, I would also
> like suggestions for place to buy copper anodes,
> stands...plating related equipments and accessories.
> Please reply to my email only. Thanks.
>
>
>
> __________________________________
> Do you Yahoo!?
> Yahoo! Mail is new and improved - Check it out!
> http://promotions.yahoo.com/new_mail
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group