Dear Colleagues,
  I worked on the microfluidic devices. When I use plasma treat the PDMS
and SU-8 (on a glass slide) sample, and try to attach them. The attachment
seems very strong at the beginning. I can even break the PDMS without
getting PDMS detached from the SU-8 layer. But when I inject the water or
put the device into the water for about 24 hours, which is typically my
experiment period, the PDMS and SU-8 are detached from each other. Does
that mean the water is able to attack the bonding between PDMS and SU-8? Do
you have any suggestion on how to improve the bonding?
  Thanks a lot!


  Sincerely,
  Jason



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing