PDMS to metal bond and corona discharge
2004-08-22
Rick Giuly
2004-08-23
Virginia Soares
2004-08-24
Michael D Martin
PDMS to metal bond and corona discharge
Rick Giuly
2004-08-22
I'm patterning a gold electrode array onto PDMS.

A paper by Yongman Park [1] presents a method that gives good adhesion. You
pattern the metal on glass and then stick it to a PDMS layer.

The paper says to expose the PDMS to corona discharge. How do you do that? Why
do you do that? Is it the same as exposing to oxygen plasma?

The paper also says treat the metal on glass with
3-mereaptopropyltrimethoxysilane (3-MPTMS) in ethanol solution, but it doesn't
say why. Why would you do that?



[1] Metal Thin-Film Micropatterns Transfer on PDMS and its Application to
Capillary Electrophoresis Electrochemical Detection on PDMS Microchip.
Yongman Park
7th International Conference on Miniaturized Chemical and Biochemical Analysis
Systems

-Rick Giuly
 GA Tech Laboratory for Neuroengineering

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer
Addison Engineering