Karin Buchholz
2004-09-02
Kenneth Smith
2004-09-03
newman
2004-09-02
Kasman , Elina
2004-09-03
Dekker, R. (Ronald)
Removing sawing residues from Si surface
Karin Buchholz
2004-09-02
Dear all,

I cut a fresh wafer into pieces using a diamond wafer saw and distilled
water. However I did not cover the surface to protect it from dirt.

What is the best way to remove the residues from the Si surface without
roughening it? For the application of biological layers I need really
smooth surfaces.

Right now I am trying DI water in an ultrasonic bath, but this seems not
efficient enough...

Any helpful tips are greatly appreciated!

Thank you, Karin

--
Walter Schottky Institut
Technische Universitaet Muenchen



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering