Can PMMA form 30nm thin film on Si substrate?
2004-09-03
Z. Jiang
2004-09-03
Yilei Zhang
Can PMMA form 30nm thin film on Si substrate?
Yilei Zhang
2004-09-03
Hi  jiang:
you may like to dilute the PMMA and try different spin speed and time.
Microchem has a list of coating thickness VS spin speed and time. that can be
a good start point.



Regards,
Yilei Zhang








reply