Hi Oray, everyone

You can use methane/hydrogen/argon to etch GaAs in ICP or RIE.  It does have
some disadvantages over chlorine containing mixtures.  It will operate at a
higher DC bias (which can leave ion bombardment damage on the etched
regions), gives a rougher surface and deposits carbon based deposits in the
chamber which have to be regularly cleaned to avoid particulates.  It has a
maximum etch rate of around 45nm/min in RIE.

Adding chlorine, either as Cl2 or BCl3 or SiCl4 avoids these problems but
then gives difficulties of handling toxic gases.  This means you must either
use a load-locked machine or use a glove box on an open load machine.  There
are other issues with gas lines, continuous monitoring for leaks etc.

Also, while CH4/H2/Ar will etch GaAs, it will not touch anything containing
Al (such as AlGaAs).

Feel free to contact me direct by email at [email protected] if you
need more information.

Martin

---------------------------
>
> Message: 3
> Date: Mon, 20 Sep 2004 19:10:43 +0300
> From: Oray Orkun Cellek 
> Subject: [mems-talk] RIE gases
> To: [email protected]
> Message-ID:
>       <[email protected]>
> Content-Type: text/plain; charset=iso-8859-1
>
> Dear Mems-Talk users,
>
> For safety reasons we plan to establish an RIE system that uses safe
> CH4/H2/Ar plasma for etching GaAs and other compund semiconductors.
>
> I wonder what is the disadvantage of this chemistry when compared to
> the popular and toxic BCl3 and SiCl4 ?
>
> Can you compare these in terms of etch rate and isotropy for an
> ordinary RIE system ?
>
> Does CH4/H2/Ar really demand RF supply systems like ICP or ECR ?
>
> Thank you in advance,
>
> Best Regards,
>
> Oray Orkun Cellek
> Research Assistant, Ph.D. Candidate
> Electrical & Electronics Engineering Department
> Middle East Technical University
> 06531
> Ankara, Turkey
> e-mail : [email protected]
> Tel : +90 312 210 4579
> Fax: +90 312 210 1261
>


 ###  OXFORD INSTRUMENTS   http://www.oxford-instruments.com/  ###

Unless stated above to be non-confidential, this E-mail and any
attachments are private and confidential and are for the addressee
only and may not be used, copied or disclosed save to the addressee.
If you have received this E-mail in error please notify us upon receipt
and delete it from your records. Internet communications are not secure
and Oxford Instruments is not responsible for their abuse by third
parties nor for any alteration or corruption in transmission.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.