MEMSnet Home: MEMS-Talk: pH in CMP Clean
pH in CMP Clean
2004-09-29
Booth, David
2004-09-29
Gary
pH in CMP Clean
Gary
2004-09-29
Use Amonia to raise the pH. Gary

Gary Hillman
Service Support Specialties, Inc.
9 Mars Court
PO Box 365
Montville, NJ 07045
973-263-0640
973-263-8888.



-----Original Message-----
From:   Booth, David [SMTP:[email protected]]
Sent:   Wednesday, September 29, 2004 1:43 PM
To:     [email protected]
Subject:        [mems-talk] pH in CMP Clean

Can anyone suggest a better method of increasing the pH during sapphire
polishing than KOH, using a SiO2 slurry and needing a pH of 10-11?
Thanks very much.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation