Hi there,
I have performed in the past SiO2 (grown and deposited on silicon wafers)etching
with all the most used technologies.
Now I am working with Soda-Lime glasses and I need to find a way to etch this
glasses with a slow rate (not more than 1 um per minute) and with a smooth
etched surface.
Any suggestions?

Thanks

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.