MEMSnet Home: MEMS-Talk: Cleaning procedure for alumina wafers
Cleaning procedure for alumina wafers
2004-10-07
Jeff Campbell
2004-10-07
Gary
Cleaning procedure for alumina wafers
Gary
2004-10-07
Jeff, What are you trying to remove from the surface of the alumina, what
kind of surface roughness exists, is the alumina at or near theoretical
density.  Those questions need to be answered to answer yours.  Gary

Gary Hillman
Service Support Specialties, Inc.
9 Mars Court
PO Box 365
Montville, NJ 07045
973-263-0640
973-263-8888.



-----Original Message-----
From:   Jeff Campbell [SMTP:[email protected]]
Sent:   Thursday, October 07, 2004 10:59 AM
To:     General MEMS discussion
Subject:        [mems-talk] Cleaning procedure for alumina wafers

Hello,

Does anyone have a good cleaning procedure for cleaning alumina wafers?
For now we are just using a solvent clean.

thanks to all,

Jeff Campbell
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group