MEMSnet Home: MEMS-Talk: Leakage test
SU-8 Chemical Resistance
2004-10-29
Srinivas Parimi
Leakage test
2004-10-31
rakesh babu
2004-11-01
Kirt Williams
EM simulation
2004-11-02
piyush tilloo
Leakage test
Kirt Williams
2004-11-01
You might be able to look with an IR microscope.

----- Original Message -----
From: "rakesh babu" 
To: "General MEMS discussion" 
Sent: Saturday, October 30, 2004 5:29 PM
Subject: [mems-talk] Leakage test


> folks,
>
>   How can i test whether a liquid trapped inside a
> surface micomachined chamber has leaked through one of
> the etch holes or has evaporated.
>
>  Thanks a lot.
>
> Sincerely
> Rakesh Katragadda


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review