MEMSnet Home: MEMS-Talk: TMAH Etch Without Attacking Aluminum
TMAH Etch Without Attacking Aluminum
2004-11-22
Kevin Duan
2004-11-23
Z.,W.Y.(Lydia)
TMAH Etch Without Attacking Aluminum
Kevin Duan
2004-11-22
Hi, dear all

I am planning to do TMAH etching of silicon wafer with aluminum
pattern on it.  I want to achieve as low etch rate for Al as possible.
 Some people add some silicon powder and some other additive, like
amonium nitrate to do that.  Does anyone have some experience in doing
so?  How about the experimental setup and the condition?

Thanks ahead.

Duan

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics
Nano-Master, Inc.