A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to find the suitable gap between the contacts.
How to find the suitable gap between the contacts.
2005-01-11
hare krishna
How to find the suitable gap between the contacts.
hare krishna
2005-01-11
Dear All,
   I need to measure the schottky barrier height. For
this I have to have a central schottky contact
circular pad and then some gap and then an ohmic
contact(so the final structure would be two metal
contacts of different metals separated by a ring gap).
I have to find the suitable gap between the contacts
such that the schottky contact resistance will
dominate compare to series resistance between the
contacts(schottky and Ohmic). I have to do some
simulation for this. How should I proceed. What are
the equations I have to consider for the same.
Any suggestions will be appreciated.
Hare Krishna










__________________________________
Do you Yahoo!?
Yahoo! Mail - now with 250MB free storage. Learn more.
http://info.mail.yahoo.com/mail_250

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing