MEMSnet Home: MEMS-Talk: Help: RIE with small feature size
Help: RIE with small feature size
2005-01-25
xiaodong wang
2005-01-25
Isaac Wing Tak Chan
2005-01-25
Michael D Martin
Help: RIE with small feature size
Isaac Wing Tak Chan
2005-01-25
Dear Xiaodong,

SF6/O2 is a very isotropic process. I suggest you try SF6/Ar for starter.
Keep SF6 around 10% of gas flow. Yes, it will be somewhat reactive sputter
etching. Can you cool your substrate to cryogenic temperature in your RIE
system? You may not want polymerization using CxFy gases to form on the
sidewall for your small feature size because your etching may halt at some
trench depth as your polymer closes up the neck of the trench.


Yours sincerely,

Isaac Chan
University of Waterloo

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation