Hello,

I am  a french student working on z-cut quartz etching.
I'd like to etch a 500µ (to have a 30µ structure) wafer but I can't
obtain a
good smoothness
(using 48% HF and 40% NH4F at 18°C).
Maybe somebody could help me!

thx

_________________________________________________________________
MSN Actions Solidaires : volontaire à l'étranger
http://www.msn.fr/actionssolidaires/Default.asp?Ath=f


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics