MEMSnet Home: MEMS-Talk: Re: solubility of PMMA
Re: solubility of PMMA
2005-02-23
Harald Walter
2005-02-23
[email protected]
Re: solubility of PMMA
Harald Walter
2005-02-23
Dear Yu,

you will find some information here:
http://www.ahlborn-kunststoffe.at/english/databaseframe.html
Assuming you want the PMMA to be stable, methanol is
bad and HCl ok at RT.

Another good source for data on polymers is:
http://www.goodfellow.com/csp/active/gfHome.csp

Harald