MEMSnet Home: MEMS-Talk: PDMS thickness variation with spin speed and time.
PDMS thickness variation with spin speed and time.
2005-03-15
Kapil Sahasrabudhe
2005-03-15
[email protected]
2005-03-15
Gary
2005-03-15
[email protected]
2005-03-16
[email protected]
2005-03-16
[email protected]
2005-03-16
[email protected]
2005-03-16
Kapil Sahasrabudhe
2005-03-15
Z.,W.Y.(Lydia)
2005-03-16
karim faid
2005-03-17
Z.,W.Y.(Lydia)
PDMS thickness variation with spin speed and time.
[email protected]
2005-03-16
Use Su-8 and make the PDMS stamp off of it.

> I have been atempting to make a microfluidic structure out of SU-8 and
> just
> this week I was going to try working with that same line of PDMS instead,
> so if
> anyone has any literature or technique suggestions for spinning and
> processing
> PDMS structures (mine will be approx 50 microns thick), I would appreciate
> it
> as well.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics