A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Selectivity of PR, SiO2, Si3N4 to Si in DRIE process
Selectivity of PR, SiO2, Si3N4 to Si in DRIE process
2005-05-10
Pradeep Dixit
Selectivity of PR, SiO2, Si3N4 to Si in DRIE process
Pradeep Dixit
2005-05-10
Dear All,

I want to etch 450 um thick wafer with 20 micron hole in STS DRIE
process.  Which kind of mask i should use ? I have not good results
with 10 um thick AZ9260 photoresist mask.

Will some one tell me what is the selectivity of Photoresist to Si,
SiO2 to Si and Si3N4 to Si in DRIE process.

--
Thanks,
Pradeep Dixit
Research Student,
Micromachine Center,
NTU Singapore - 639669
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation