MEMSnet Home: MEMS-Talk: Au Thickness vs. Conductivity
Au Thickness vs. Conductivity
2005-05-23
Mr Edward Keough
2005-05-24
John Maloney
2005-05-24
MT Klaus Beschorner
Au Thickness vs. Conductivity
John Maloney
2005-05-24
> does anyone have a reference or chart for the film thickness
> of Au. and
> its conductivity (electrical). I would like to know how thin
> (<100nm)I
> can go before I start to lose conductivity throughout the
> entire film.
> I am depositing on glass with a 10nm Ti adhesive layer.

Hi Ed,

   Check Koch et al, "Resistivity-noise measurements in thin gold films
near the percolation threshold" in Phys Rev B, 32(10), 1985.  Note that
the resistance-thickness relationship will be strongly affected by
surface conditions, including the adhesion layer material and
microstructure.  The results in your lab may not match literature
reports.  Hope this helps,

John Maloney
MicroCHIPS, Inc.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering