MEMSnet Home: MEMS-Talk: si etch help
si etch help
2005-05-27
babitha bommalakunta
2005-05-27
[email protected]
2005-05-28
Daniel Lloyd
si etch help
Daniel Lloyd
2005-05-28
Hi,

I've had a similar effect- it appears as rings which vary in density and
width. The main cause does seem to be heat build up in the sample- I've
found that several shorter etches reduce the problem, but need to find a
lower power recipe (or to increase my sample cooling).

Regards,
Daniel

-----Original Message-----
From: babitha bommalakunta [mailto:[email protected]]
Subject: [mems-talk] si etch help

I am trying to work out Si etch process with CF4 and O2 combination in pecvd
system.My sample appears white after etching . Any idea due to what this
happens?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review