MEMSnet Home: MEMS-Talk: RE: Spam:[mems-talk] Low refractive index optical polymer
RE: Spam:[mems-talk] Low refractive index optical polymer
2005-06-21
Matthew Coda
RE: Spam:[mems-talk] Low refractive index optical polymer
Matthew Coda
2005-06-21
There is a DuPont compound with in index below 1.32 called AF 1600; it
can be spin coated.  I believe the index is tunable by the addition of
other fluorinated or semi-fluorinated compounds.

Good Luck,
Matt Coda