A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Thin PDMS Films
Reg: problems with SU-8 bonding to the silicon wafer
2005-06-23
Vishwanath Somashekar
2005-06-23
[email protected]
2005-06-23
Vishwanath Somashekar
Thin PDMS Films
2005-06-24
[email protected]
2005-06-25
Tolga Kaya
2005-06-27
Patrick Roman
2005-06-23
Brubaker Chad
2005-06-24
Brubaker Chad
2005-06-27
Vishwanath Somashekar
2005-06-29
Brubaker Chad
2005-06-30
Vishwanath Somashekar
Thin PDMS Films
[email protected]
2005-06-24
Hi all,

I was wondering if anyone has experience casting thin films of PDMS by
clamping down the mold in order to get a film that is as thick as the features
on the mold. If so, does anyone have suggestions/tips on removing the film
from the mold once it's done? I've been having trouble with tearing the film
as I try to peel it off by hand.

thanks,
Joe Grogan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.