Aluminum etch
Brent Garber
2005-07-06
Arvind,

Transene makes fine etchants as do other companies.  I have also used 10% HNO3
90% H3PO4.

Brent

Arvind Balasubramanian wrote:

> Hello all,
>
>     Iam new to MEMS talk and its a pleasure to mail the group. I would like to
know if anyone had wet etched aluminum. If so, can you please help me in
choosing a etchant. I was looking at Transene Aluminum Etchant. Have anyone used
this etchant?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group