Hello,

Is there anyone who know how to erease the seed layer of Au after Nickel
electroplating? We found that after plating, Au is harder to erease in KI
etchant. The problem is that it is impossible to add an additional layer of
photoresist to protect the nickel. After long time etching, the nickel is
also etched away.

Thanks a lot,

X.Y. Ye