maryala shivakumar
SiO2 over gold
2005-08-03
mojgan daneshmand
2005-08-03
Richard Chang
2005-08-04
Jesse D Fowler
2005-08-03
Guillermo Villanueva
SiO2 over gold
mojgan daneshmand
2005-08-03
Hi everyone,

I am having problem with PECVD SiO2 over gold film. Our oxide film looks
perfectly fine over any surface rather than gold. It cracks over any gold
pattern. Has anyone seen any similar problem? any idea how I can fix the
problem?

Thanks to everyone.
Mojgan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.