MEMSnet Home: MEMS-Talk: Resist as paste
Resist as paste
1998-06-26
Christophe Sudre
Resist as paste
Christophe Sudre
1998-06-26
Hi everybody

I'm going to do some process with SiC wafers. The problem is the machine
I can use are designed for 4 inch wafers .. and my SiC wafers are 1.3
inch cutted in four !!! For the sputter deposition machine, no problem,
I can use a metal wafer with clips to fix the little wafer. For the
implanter, I can't use that and I must stick the wafer on a 4 inch Si
wafer. The only way I see is to use resist. Do you have other ideas ?
Did somebody use resist as paste ? How did you that ?

Many thanks per advance, Christophe Sudre

--
 _______________________________________________________________________________
| Dr Christophe Sudre                             Fax :   353 21 270271
|
| Research Scientist                              Phone : 353 21 904079
|
| University College Cork                         WWW :
http://www.nmrc.ucc.ie/|
| National Microelectronics Research Center       Email: [email protected]
|
| Lee Maltings, Prospect Row
|
| Cork, Ireland
|
|_______________________________________________________________________________
|


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Nano-Master, Inc.
Tanner EDA by Mentor Graphics